Charpy V-Notch Impact Testing at -60°C: What to Require

Quality & inspection

Charpy V-Notch Impact Testing at -60°C: What to Require

Charpy V-notch testing at −60 °C needs 10×10×55 mm specimens, 3 per heat, and energy limits set by GOST 32400-2013 or the buyer. Learn what to specify.

Published: · Last updated: · Reviewed by Wang Jingchun

For cold-climate railway castings, specify Charpy V-notch impact tests at −60 °C using 10×10×55 mm specimens with a 2 mm notch, taken 3 from each heat lot and tested at the specified temperature. GOST 32400-2013 sets the envelope for 18-100 side frames and bolsters, while AAR M-201 leaves the exact energy limit to the purchaser. SIMIS casts test coupons attached to the heat so results represent the actual pour.

What to Specify for Charpy V-Notch at −60 °C

RequirementTypical specification
Specimen10×10×55 mm, V-notch 2 mm (ASTM E23 / ISO 148)
Test temperature−60 °C (sub-size coupons at −40 °C where allowed)
Specimens per heat3 (report average and individual)
Acceptance energySet by GOST 32400-2013 or buyer's purchase order
Coupon locationAttached to the casting heat, same pour

State the temperature and the minimum absorbed energy on the drawing and the purchase order. A standard such as AAR M-201 defines the grades but leaves the impact value to the purchaser, so the number that matters is the one written on your order, not a generic table value.

Test Method and Standard Requirements

Charpy V-notch testing measures the energy a notched specimen absorbs at fracture. ASTM E23 and ISO 148 define the pendulum machine, specimen geometry and the −60 °C bath control. GOST 32400-2013, effective 2014-07-01, governs cast-steel bogie parts — specifically side frames and bolsters — for the CIS market and sets low-temperature toughness requirements that the purchaser applies through the purchase order. Where AAR M-201 applies, the impact value is a purchaser-specified requirement rather than a fixed number in the standard. The key is to state the temperature and the minimum absorbed energy on the drawing and the PO so the foundry and the third-party inspector read the same limit.

Coupons, Equipment and Production Control

The impact coupon is poured from the same ladle as the castings and heat-treated with them, so its result represents the actual component material. SIMIS attaches coupons to the heat, machines them after heat treatment, and tests on a calibrated pendulum machine with a verified low-temperature bath. The EBT+LF duplex refining keeps sulphur and inclusions low, which directly supports stable low-temperature toughness. Test temperature is held within ±2 °C and the machine is verified with reference specimens before each batch.

Acceptance, Certification and Traceability

The Charpy results are recorded on the factory material certificate, fully compliant with EN 10204 3.1 against the heat number, together with the tensile and chemistry results. Each casting is marked with the heat number and a serial number, so a low-temperature failure in the field can be traced to the exact coupon and pour. SIMIS retains the test records for the contract period and supplies the material certificate with the shipment.

Frequently Asked Questions

What specimen size and test temperature should be specified?

Specify 10×10×55 mm V-notch specimens tested at −60 °C per ASTM E23 or ISO 148, with sub-size coupons used only where the standard and buyer permit. State both the temperature and the minimum absorbed energy on the drawing and purchase order, because AAR M-201 and most standards leave the exact energy limit to the purchaser rather than fixing it.

How many specimens per heat lot are required?

Take three specimens from each heat lot, poured and heat-treated with the castings, and report both the individual values and the average. GOST 32400-2013 and typical purchase orders require this three-specimen set so a single outlier does not condemn a heat; the disposition follows the buyer's acceptance criteria and the recorded average.

Why do buyers request impact test coupons with the casting?

A coupon poured from the same ladle and heat-treated with the castings proves the actual component material, not just a ladle sample. This matters for −60 °C service where toughness varies with chemistry and cooling. The coupon result is tied to the heat number on the factory material certificate, fully compliant with EN 10204 3.1, giving traceable evidence for field failures and third-party inspection.

Request a Quotation

Send your drawing with the required grade, test temperature and minimum impact energy to sales@simisrail.com. SIMIS confirms receipt within 1 working day and returns a quotation with indicative lead time and MOQ, including coupon and testing scope.

Technical Review

For a question on the Charpy V-notch test, contact Felix at sales@simisrail.com or +86-13934165890.